Styrene Binder-1 Formula

Component dosage /g component dosage /g
SBR 100 Antioxidant Ding 3.2
Zinc oxide 3.2 carbon black amount
Sulfur 8 dibutyl phthalate 3.2
Accelerator DM 3.2 Xylene 1000   
Preparation and curing    Curing for 30 minutes at 148 °C .
Use The glue is used for the bonding of rubber and metal and the bonding of rubber products.