Gravure Common Faults - Bad Plastic Print Fastness

The reasons for poor fastness of plastic film printing are as follows:

1. The corona treatment of the polyolefin film was poor.

Countermeasures: Check whether the surface tension of PE and PP reaches 40 dynes/cm or more.

2. The printed ink and printed material have poor affinity. This is a poor mixture ratio. Countermeasures: Replace the ink and adjust the solvent ratio.

3. The printing shop temperature and relative humidity change greatly.

Countermeasures: As far as possible, the relative humidity of the workshop should be controlled between 50% and 60%, but it should not be too low. Below 40%, it is easy to generate static electricity. The best room temperature is controlled at 18 °C ~ 23 °C for the best, and keep the environment clean and air circulation.

4. The plastic film itself is extremely poor in printability and is still undesirable after corona treatment.

Countermeasure: Replace the printed material.

Glass Concentrate Containers


Child Resistant Glass Concentrated jars are getting quite popular.
Glass container jars are classy, durable, and can resist both moisture and liquids. They can store wax, oils, and dry canna without any damage to the products.Made of high quality glass,it doesn't get corroded or reacts with the canna product inside. It will ensure that your product does not get contaminated.The non-degrading nature of the concentrate jars packaging also makes them a long-life solution. You can use them to store products for years without any trouble.

Child Resistant Concentrate Containers , Child Resistant Packaging Tube, Child-Resistant Concentrate Jars, Glass Concentrate Jars ,Concentrate jars packaging

NANTONG OUFEIYA IMP& EXP CO.,LTD , https://www.jsnantongoufeiya.com

Posted on